Click on the pictures for a full size image in a new window.
| | A rack with 3 damaged teeth. |
|
| | The same rack after silver soldering a piece of steel into place and filing 3 new teeth. |
|
| | Broken glass pendulum vials |
|
| | New mercury filled vials fitted to the pendulum. |
|
| | A fractured hour wheel pipe. |
|
| | A new pipe was turned on the lathe and soldered into place. |
|
| | A bodged repair comprising of a plate pinned over a worn hole |
|
| | The plate removed and a bush fitted. |
|
| | A worn pivot hole |
|
| | A bush inserted in the hole and broached to size. |
|